Abstract
The kinetics of degradation of polysiloxanes with different starting chemistries is reported in this paper. The polymers used in the study were vinyl-terminated polydimethylsiloxane (PDMS) and poly(diphenyl-dimethyl)siloxane (3.5 and 25% diphenyl content, DP-3.5 and DP-25). These polymers were inert pyrolyzed under isothermal conditions at temperatures from 325 to 400 � C for 5 h. Additionally, these polymers were pyrolyzed under dynamic heating (rate 6.25 � C/min) up to 925 � C. The kinetic rate constants were calculated for each of the polymers, from both isothermal TGA and dynamic, non-isothermal TGA. The Van Krevelen and Coats-Redfern methods of analysis were used for calculating the energy of activation from dynamic TGA. The various analysis